Design and Process Integration

Integration. Design and Process Integration. Overview. Integration Matching/ Accommodating different processes to obtain a ‘passing’ or good chip Process Integration Design/ Process Integration Modifying the design (slightly), to suit the process

bernicek
Télécharger la présentation

Design and Process Integration

An Image/Link below is provided (as is) to download presentation Download Policy: Content on the Website is provided to you AS IS for your information and personal use and may not be sold / licensed / shared on other websites without getting consent from its author. Content is provided to you AS IS for your information and personal use only. Download presentation by click this link. While downloading, if for some reason you are not able to download a presentation, the publisher may have deleted the file from their server. During download, if you can't get a presentation, the file might be deleted by the publisher.

E N D

Presentation Transcript


  1. Integration Design and Process Integration

  2. Overview • Integration • Matching/ Accommodating different processes to obtain a ‘passing’ or good chip • Process Integration • Design/ Process Integration • Modifying the design (slightly), to suit the process • Usually, the electrical circuit is not altered • Assumes that process has been developed or optimized to the maximum possible extent • Always remember that the cost /benefit is the ‘bottom line’

  3. Index • Miscellaneous • Electro migration • Scaling in MOS • Electrical Structure (mostly FEOL) • BEOL Cu vs Al and Low-K vs Oxide

  4. Electro migration • Due to movement of electrons, the atoms in a very small line move • formation of voids, increase in electrical resistance, complete breakdown • hillocks, whiskers ==> shorts • Minimum length needed “Blech Length” for a given current density • Depends on the material • Copper, Gold good electromigration resistance • Reliability issue

  5. Electro migration • Mean Time to Fail (MTF) depends on Current Density (J) • Current Density few million Amp/sq cm • Grain size: • movement along grain boundaries faster • For very small lines, grain size = line width • if av grain size is 1 um, a 10 um line will fail quickly (for the same current density, a 1 um line will fail later, a 0.5 um line may fail more quickly) • also depends on arrangement and orientation of grain

  6. Electro migration • Al is more prone to electromigration, however... • Cu does not form a stable strong oxide • Delamination from the liner is an issue • EM failures in copper likely to be in the interface, in Al, in the bulk • Also, W has very high resistance to electromigration • Length of a path may not become very high • In Cu, (especially with dual damascene), for the same design, length may become more

  7. Reliability • Infant Mortality regime (components of poor quality) • Working life Regime • Wear Out regime Fail/unit time • Arrhenius equation • High Temp Operation Test - HTOT • Highly accelerated Stress Tests (HAST): - high humidity, high temp Time

  8. Reliability • Different mechanisms of fail may have different activation energies • ==> Bimodal distribution of fails Cumulative % Fails Temp • Arrhenius equation is suitable for chemical reactions • Not always suitable for explaining physical failure mechanisms

  9. Scaling • Scaling: If you reduce all the features (or some set of parameters) by a constant factor, will the performance be similar? Better? Worse? • Eg. Important dimensions are TOX, L, X L Gate TOX Source Drain X Depletion Region

  10. Scaling • Information from W. Maly: Atlas of IC Technologies • If all dimensions are reduced by 2 (for example) CS0 CS L/2 TOX/2 Gate X/2 X/2 • With same diffusion process, to obtain a shallower junction, need to start with lower initial concentration • ==> very high sheet resistance (shallow Jn, low dopant)

  11. Scaling • If only some dimensions are scaled • eg. TOX and L, but not Junction depth CS0 L/2 TOX/2 Gate X X • Depletion regions merge, short channel

  12. Scaling • If dimensions are scaled and dopant concentration “increased” CS CS0 L/2 TOX/2 X Gate X/2 X/2 • Tolerable sheet resistance • ==> High gradient of dopant in the Jn (hot electron effect) ==> LDD etc

  13. Scaling • Constant Field : • Reduce a physical dimension by ‘k’ , then reduce the voltage also by k • This reduces drain current, gate delay and gate-channel capacitance by k • Number of circuits/ sq cm increases by k2

  14. Scaling • Power per unit area remains constant • in CMOS. NMOS and Bipolar do not follow this scaling rules ==> Issues • Power Delay product (PDP) • NOTE: Total power, not power per unit area: • Reduces by cubic • Practical Limitations by processes (eg. Litho resolution, alignment, process marginalities)

  15. Metal Gate • MOS: using metal gates: Gate oxide etch/growth N N Si N N N N Source/Drain Diff and oxide growth Contact Etch

  16. Metal Gate Gate Source Drain N N N N Metal Dep Metal Etch • Minimum Feature Size is 2l • Alignment tolerance l • Based on the above steps, only 5% of the area is used for transistor channel • Overlap of gate to source and gate to drain ==> capacitance

  17. Poly Gate • MOS: using poly gates: • Active Mask (STI for example) • Poly dep/etch/ implantation (self aligned) • Contact formation • --- Withstands high temp • Active channel area is about 12% of total area • lower capacitance • better channel definition • one more interconnect layer (poly)

  18. Electrical Structures • Electrical Structures: • Resistor: • Poly (silicided) for low resistance and unsilicided for high resistance • silicided: 5 to 10 ohm/square • unsilicided 300 to 500 ohm/square (depends on dopant level and type) • undoped silicon (intrinsic) very high resistance, not usually used • Can be ‘created’ during gate formation

  19. Electrical Structures • Active (source/drain) areas can also be used for high resistance • Ohmic vs Schottky contact for lightly doped n structure • P type or highly doped N type • CAPACITOR: • MOS capacitor, similar to transistor • In the BEOL in some cases (Metal Insulator Metal Capacitor ) (Use Al for better thickness control) • Deep Trench capacitor (FEOL) for DRAM

  20. Electrical Structures • INDUCTOR: • Metal ‘circle’ • Inductance related to number of turns, radius etc • Parasitic resistance, capacitance • BEOL • Diode: • PN Junction diode • Schottky Diode • high reverse bias current • Many ‘slotted’ N+ in P well, with merging depletion region, for good reverse bias current (appears as PN in reverse, as Schottky in fwd)

  21. FEOL Flow-I • Review • Sequence with more detail than what we saw before • Start with bulk P type silicon • Oxidize and strip (obtain clean surface) • Pad oxide and Nitride • Trench Lithography • Active (source drain) and gate area definition • CD measurement for example • Trench Etch • post etch CD measurement • etch bias

  22. FEOL Flow-II • Trench Etch • blind etch • less than a micron depth • post etch CD measurement • etch bias

  23. FEOL Flow-III • Trench oxidation (very small thickness) • TEOS Dep (0.5 micron for example, above active)+ Anneal • Reverse Active Mask: Litho, etch (about 0.5 micron) • To reduce the ‘load’ on STI CMP • load here means planarization load, NOT the removal load • STI CMP • target 0.5 micron removal on small active (faster polish area) for example • Other integration LOCOS • OR modification of STI by Poly Dep+CMP .... • Nitride Removal

  24. FEOL Flow-IV • Pad oxide removal • Sacrificial oxidation (10 nm) • Nwell implant • Pwell implant • Gate Oxidation • Poly deposition (perhaps thin cap oxide for hard mask) • Gate Litho(use ARC)/ Etch • NMOS implant (LDD, Halo): Not the main implants • PMOS implant (LDD, Halo): Not the main implants • RTP

  25. FEOL Flow-V • Spacer Formation • Nitride • Spacer etch • NMOS (main) implant • PMOS (main) implant • RTP • If you need unsilicided areas, you need to mask them with oxide/nitride • Pre-silicide clean (eg. Sputter the surface, or light chemical etch) • Co dep • Anneal (about a minute, 500 C) • Un-reacted Co removal • Nitride Dep (for contact etch)

  26. FEOL / BEOL • BPSG Dep + Anneal + CMP (0.5 um thick remaining) • Cap Ox (to withstand W CMP in the next steps) • Contact photo + etch • Ti/TiN Liner dep (IMP Ti, CVD TiN) • W CVD • W CMP • ILD/PMD Oxide for Copper, Barrier Dep for Al

  27. BEOL (Aluminum) • Barrier Dep (Ti/TiN) • Al Dep (PVD) + Ti/TiN • Al Photo + Etch (M1 levl) • Oxide Dep • Oxide CMP (blind) • Via12 etch and so on...

  28. BEOL (Copper) • Oxide Dep • M1 photo + Etch • Liner (Ta/TaN) Dep • Cu (seed + electrochem) Dep • Cu CMP • Nitride (via etch stop layer) dep • Oxide Dep • V12-photo + etch (stop on nitride) • M2 photo + etch (blind) and so on... • OR M2 photo + blind etch followed by V12-photo+ stop on nitride etch

  29. BEOL (Copper) • Via first integration • Resist removal from the bottom of via can be an issue • Metal first integration • Resist pooling an issue • Some Other schemes: • Single damascene • Intermediate (stop on) nitride • increased cost, lower throughput

  30. BEOL Integration • Some Issues: • Over etch: defectivity • under etch: opens • etch uniformity (center edge) • CMP • In Copper CMP, too much dishing/erosion ==> oxide needs to be planarized • increased cost

  31. Low -K • Oxide vs Low K • For RC delay reduction • Need • thermal stability • chemical inertness (selective etch) • mechanical strength (for Cu CMP) • adhesion to barrier • low stress • Thermal expansion matching • low diffusivity of contaminants (or copper)

  32. Low -K • Only if k < 3, it is considered as ‘real low-k’ • FSG (fluorinated silicate glass) (k=3.5) • not very low • absorbs water (can create HF and hence havoc) • Carbon Doped Silica (k = 3) • commercial: AMAT Black Diamond , NOVELUS Coral • uniform carbon doping is an issue • Organic polymers • low k, but soft (mechanical strength), temp stability, chemical reactivity (photoresist etc) • thermal expansion mismatch ==> crack

  33. Low -K • Organic polymers • low k, but soft (mechanical strength), temp stability, chemical reactivity (photoresist etc) • thermal expansion mismatch ==> crack • low thermal conductivity ==> more stress on metal • Adhesion, Delamination • eg. PTFE adhesion, delamination during CMP • Absorbance of chemicals during process • and subsequent release • --> metal lines and transistors affected • DLC (diamond like carbon) • etch etc not tested

  34. Low -K • Porous silica (or other materials) • Thermal, chemical stability is good • Diffusion of materials is high • Mechanical strength (CMP) may be an issue • Absorbance of chemicals an issue • Good thermal insulator ==> very high stress on metal • --> need to take heat conduction path in design • Repeatability (of process and material quality) etc need to be tested • New material: Not tested very well yet

  35. Low -K • CAP layer used to ‘increase’ mechanical strength • eg SiC. (Has high K, so only very thin films can be used) • DLC may also be used