An Image/Link below is provided (as is) to download presentation Download Policy: Content on the Website is provided to you AS IS for your information and personal use and may not be sold / licensed / shared on other websites without getting consent from its author. Content is provided to you AS IS for your information and personal use only. Download presentation by click this link. While downloading, if for some reason you are not able to download a presentation, the publisher may have deleted the file from their server. During download, if you can't get a presentation, the file might be deleted by the publisher.

E N D

Presentation Transcript


  1. COMPARATIVE WET AGEING TESTSOFMEDIUM VOLTAGE XLPE CABLES ICC Meeting - May 1, 2002Colorado Springs Hans Schädlich (Retired) - Nexans Germany Lauri J. Hiivala - Nexans Canada

  2. AC Breakdown Strength of 20 kV XLPE CablesBefore and After Ageing (Alcatel Method)

  3. VDE

  4. AC Breakdown Strength of 20 kV XLPE CablesBefore and After Ageing (VDE Method)

  5. AC Breakdown Strength of 20 kV XLPE CablesBefore and After Ageing (Accelerated vs. Service)

  6. AEIC

  7. 1250 1000 750 500 250 0 AC Breakdown Strength of 15 kV XLPE CablesAfter Ageing According to VDE and AEIC