Recipe. IngredientsPrecondensed silica (Silbond H-5, TEOS, or equivalent)Catalyst (ethanol, water, aqueous ammonia or protic acid)ProcessPlace material into autoclave filled with ethanolPressurize at 750-850 psi with CO2