Burnt-out is a process that uses two kinds of fibers with different acid resistance. After the printing and dyeing process, the burnt-out treatment is processed in an acid solution, so that the part of the fiber that is not acid-resistant is dissolved and rotten, and then, it comes to the burnt-out fabric. The main feature of the fabric is that it has a transparent, concave-convex pattern, a novel pattern, and a clear outline.