2. INTRODUCTION. MIL STD 889 precludes the use of dissimilar galvanic couples without appropriate protective systemsRecently galvanic corrosion has occurred on some newer systems and it became apparent that there was little understanding as to the impact and mechanism of such galvanic exposureTher