Quartz Crucible

Tall Form Quartz Crucible can be transparent or milky white. These quartz crucibles can withstand up to 1100 degree centigrade. It is most important to note that tall form quartz crucible can withstand very high thermal shock (1000 degree centigrade to room temperature).

Antslab
Télécharger la présentation

Quartz Crucible

An Image/Link below is provided (as is) to download presentation Download Policy: Content on the Website is provided to you AS IS for your information and personal use and may not be sold / licensed / shared on other websites without getting consent from its author. Content is provided to you AS IS for your information and personal use only. Download presentation by click this link. While downloading, if for some reason you are not able to download a presentation, the publisher may have deleted the file from their server. During download, if you can't get a presentation, the file might be deleted by the publisher.

E N D

Presentation Transcript


  1. QUARTZ CRUCIBLE Visit Our Website www.antslab.in

  2. Tall Form Quartz Crucible can be transparent or milky white. These quartz crucibles can withstand up to 1100 degree centigrade. It is most important to note that tall form quartz crucible can withstand very high thermal shock (1000 degree centigrade to room temperature). It is obtained through different types of raw materials because that includes natural or synthetic quartz sand. These are highly resistant to thermal shock due to the extremely low coefficient of thermal expansion because they have excellent electrical strength that offers stability under temperature variation. Our range of Tall Form Quartz Crucible is developed in our company by using high purity fused quartz as raw material and fabricating with advanced ceramic technology.

  3. Thermal Properties of Tall Form Quartz Crucible Thermal Conductivity 1.38(W/m°K) Coefficient Of tThermal Expansion(0~1000 °C) 0.55(10 -6/ °C) Normal Operating Temperature (Continuous Usage) ~1050 °C Normal Operating Temperature (Non Continuous Usage) ~1250 °C Strain Point ~1075 °C Annealing Point ~1180 °C Hot Pressing Temperature ~1700 °C – 2100 °C  Starting at ~1000 ° C. high temperature accelerates Devitrification, especially with surface contaminants such as alkaline solution, salts and vapours. Devitrification Temperature

  4. Physical Properties of Tall Form Quartz Crucible Units of Measure Value Density gm/cc (lb/ft3) 2.2 Porosity %(%) 0 Tensible Strength 106 Pa 48.3 Young’s Modulus 106 Pa 71.7 Hardness kg/mm2 600 Thermal Conductivity W/m°K 1.38 Coefficient of Thermal Expansion 10-6/°C 0.55 Specific Heat J/Kg°K 740 Dieletric Strength Ac-kv/mm (volts/mil)  30 Dieletric Constant @1MHz 3.82 Index of refraction @ 587.6nm — 1.4585

  5. Thank You For Your Attention Visit Our Website www.antslab.in