An Image/Link below is provided (as is) to download presentation Download Policy: Content on the Website is provided to you AS IS for your information and personal use and may not be sold / licensed / shared on other websites without getting consent from its author. Content is provided to you AS IS for your information and personal use only. Download presentation by click this link. While downloading, if for some reason you are not able to download a presentation, the publisher may have deleted the file from their server. During download, if you can't get a presentation, the file might be deleted by the publisher.

E N D

Presentation Transcript


  1. NEEP 541 – Microstructure Fall 2002 Jake Blanchard

  2. Outline • Microstructure • Definitions

  3. Defects • Planar Defects • Grain boundaries • Interphase boundaries • Twin boundaries • Domain boundaries • Stacking defaults • Volume Defects • Cavities • Precipitates • cracks • Point Defects • Vacancies • Interstitials • Impurities • Clusters • Line Defects • Dislocations • Strings of pt defects

  4. Pre-Irradiation • Point defects, dislocations, grain boundaries are key • These act as sinks and traps for moving defects • Typically in thermodynamic equilibrium Formation energy Defect concentration

  5. Pre-Irradiation • Vacancy formation energy is lower than interstitial formation energy • Equilibrium vacancy concentration greater than interstitial • Interstitials are more mobile • Dislocations not in equilibrium • Dislocation density ~1012 /m2

  6. Damage Structure • Displacements create v’s and i’s • These move by diffusion • Get recombination • …and clustering • Di-vacancies, di-interstitials • Voids • Stacking fault tetrahedra

  7. FCC interstitial configuration

  8. BCC interstitial configuration

  9. Octahedral http://www.techfak.uni-kiel.de/matwis/amat/def_en/makeindex.html

  10. Tetrahedral

  11. Lattice Effects • Interstitials deform surrounding lattice • They “share” spot with lattice atom • Called a dumb-bell configuration

  12. Di-Interstitials in FCC and BCC

  13. Dumbell - FCC

  14. Dumbell - BCC

  15. Vacancies • Produce weaker lattice deformation • Form planar and 3-D clusters • Lattice collapses around planar clusters (dislocation loops) • 3-D clusters are voids or stacking fault tetrahedra (SFT) • Impurities (inert gases) stabilize voids

  16. Dislocation loops • Lattice collapses around platelet of vacancies or interstitials • Frank loops form • Loops grow • Loops convert to perfect loop • Loops rotate

  17. Interstitial Loop

  18. Vacancy loop

  19. Loop Growth • Loops grow by collecting point defects as they diffuse • Typical growth equation is: Point defect flux to loop Thermal emission

  20. Loop Growth • Z represents preferential attractive interaction between dislocation loops and moving interstitials over that with vacancies • That is, dislocation loops are more likely to absorb interstitials than vacancies • This tends to leave an excess of vacancies in the lattice • Hence, interstitial loops tend to grow and vacancy loops tend to shrink

  21. Voids • Excess vacancies can form 3-D clusters • Usually some inert gas is needed to stabilize these voids • At low temperature (<0.25Tm), diffusion is slow so voids don’t form • At high temperature (>0.5Tm), thermal emission eliminates voids • In between, void formation is likely • This causes swelling (we’ll come back to this)

  22. Microstructure Development • 3 changes occur as damage takes place • Changes in dislocation structure • Void formation and growth • Changes in chemical state (segregation, precipitation)

  23. Destination of Au Interstitials

  24. Dislocation Changes • Dislocations change shape and size • Length increases by loop growth and interactions with other dislocations • Length decreases due to annihilation • In annealed materials, length increases • In cold-worked materials, length decreases

  25. Dislocation Density Evolution

  26. Microchemical Changes • Cascades can destroy clusters and dissolve precipitates (effective diffusion) • Increased point defect densities enhance diffusion

  27. Diffusion Coeff. for Ni alloy