An Image/Link below is provided (as is) to download presentation Download Policy: Content on the Website is provided to you AS IS for your information and personal use and may not be sold / licensed / shared on other websites without getting consent from its author. Content is provided to you AS IS for your information and personal use only. Download presentation by click this link. While downloading, if for some reason you are not able to download a presentation, the publisher may have deleted the file from their server. During download, if you can't get a presentation, the file might be deleted by the publisher.

E N D

Presentation Transcript


  1. Ni Based Superalloy:Waspalloy

  2. Background of Waspalloy • Developed by NASA on their power recovery turbine blades. • Nickel based alloy used in high heat/stress situations: • jet-turbine machinery • hot gas expanders • high temp. seals. • Extremely resistant to corrosion by combustion products, up to 1600°F.

  3. Micro Structure • Vacuum Induction Melting: VIM • Reduced levels of nitrogen and oxygen • Allows for better control of Titanium and Aluminum alloying • Increases forgeability • Produced in cast and wrought forms • FCC structure

  4. Properties • Specific Gravity- • Waspalloy - 8.25 • Steel - 7.83 • Titanium - 4.55 • Composition- • 57% Ni 19.5% Cr • 13.5% Co 4.3% Mo • 2% Fe (max) 1.4% Al • 3% Ti .07% C • .006% B .09% Zr • Waspalloy retains its original composition until 1400°F while steel falls off @ 800°F