1 / 12

Weaving calculation

Weaving calculation for Fabrics

sheshir
Télécharger la présentation

Weaving calculation

An Image/Link below is provided (as is) to download presentation Download Policy: Content on the Website is provided to you AS IS for your information and personal use and may not be sold / licensed / shared on other websites without getting consent from its author. Content is provided to you AS IS for your information and personal use only. Download presentation by click this link. While downloading, if for some reason you are not able to download a presentation, the publisher may have deleted the file from their server. During download, if you can't get a presentation, the file might be deleted by the publisher.

E N D

Presentation Transcript


  1. CHAPTER - 7 WEAVING CALCULATION & USEFUL FORMULAS: 7.1. Count: A number indicating the Mass per unit Length OR • The length per unit mass of Yarn. • Expression of the fineness of Yarn. • There are three Systems to Calculate Count - 1. Indirect System 2. Direct System 3. Universal System 1 Lea = 120 yd 1 hank 7 Leas = 840 yds. or 768 meter 1 Hank = 1. Indirect system Total No. of hanks per one pound is the count of that yarn (Ne) i.e. if 10 hanks (10 x 840 yds. or 7680 meters) weighs one Pound or 0.454 Kg, then the Count of Yarn in indirect system 10s or 10Ne. This System widely used for staple fiber spun yarns like 100% Cotton, Viscose, Polyester fibers and their blends. Higher the yarn Count i.e Ne the yarn is finer Length hanks in (840 yards) Count = Weight Pounds in 2. Direct System Count = Weight in grams per 9000 meters of yarn In this system the yarn numbering is called as Denier (D) Higher the yarn number i.e Denier the yarn is coarser. 3. Universal System Count = No of grams per 1000 meters or per km of yarn. In this system count is called as Tex

  2. Commonly used other numbering systems I. Nf - French count: - It is the No of 1000 meters length in ½ kg of yarn II. Nm - Metric system: - Count is the No of 1000 meters length per kg. of yarn. III. Worsted system: - Count is the No. of 560 yards in one lbs. IV. Linen system: - It is the No. of leas of 300 yards per pound V. Hemp, Jute, Flax: - Count is the No of 14,400 yards length per pound of yarn Conversion System English (Ne) to Denier (D) = 5315 / Ne - Denier English (Ne) to Tex - Tex = 590.5 / Ne French (Nf) to English (Ne) - English (Ne) = Nf x 1.181 7.2. Twist per Inch or meter (TPI or TPM) ? To give strength to the yarn, certain twist is given in the yarn. ? TPI vary according to end use of yarn. More twist for warp yarns, medium twist for weft yarns and less twist for hosiery yarns. ? We calculate the twist as TPI or TPM. ? Twist is given in ‘Z’ direction or ‘S’ direction. ? If twist is given in CW direction it is ‘Z’ twist. ? If it is given in CCW direction it is ‘S’ twist. ? Single yarns are given ‘Z’ twist and double yarns are given ‘S’ twist. ? Twist relation for double yarn TPI = 0.7 x Single yarn TPI 7.3. Multi-filament Yarns Multi-filament yarn are identified as 80/34/250, 80/34/0, 155/16/120 Here the first number denotes the Denier, second shows No. of filaments in the yarn & the last indicate No. of Twist per meter. 7.4. Winding Calculation Slub – catcher settings: a. Fixed Blade = Carded - (2.0 to 2.5) x Diameter Combed - (1.5 to 2.0) x Diameter b. Oscillating Blade = Smooth micro-set - 25% more than above

  3. c. Serrated Blade = 100% more than the above d. Electronic yarn clearer = 3 cm x 3 Diameter 1/ (28 x count inches ) Diameter For Blended yarn = = 10 to 15% more settings Faults remved 100 × Yarn clearer efficiency = Faults Total present breaks during winding (at faults) Knot factor = No. of objectiona to due Breaks faults ble stength of spliced joint 100 × Retained splice strength = strength of parent yarn Winding Tension = 0.1 x Single strength in grams 4.8 y × 1 + Optimum spindles / winder N = OR S 4500 Y × S N 13Y 12 98 ( ) × + Expected efficiency E = Expected production P = / Winder per 8 hrs. in kgs 12 98 ) C × ( + Y = Length / Bobbin (meters.) S = Winding speed (meters./min) B = breaks per bobbin C = English count 7.5. Warping Calculations: R 100 × Machine Efficiency E = R S + 1000× 60 R = Uninterrupted running Time for 1000 meters (sec) = Machine speed mtr/min in S = total of time, in seconds for which the machine is stopped for a production of 1000 meters. T2 400 B = End breaks / 400 ends / 1000 meters L = Set Length in 1000 meters Timing of activities in Seconds are T1 = To mend a break T2 = To change a beam T3 = To change a Creel T4 = Miscellaneous Time loss / 1000 mtrs. N B × T1 T3 × R T4 + + + + = L L C × N = Number of ends. C = Beams per creel.

  4. Production in meters. per 8 hrs.(K) = 480 x mtrs / min x E / 100 Kgs. Production in Kgs. Per 8 hrs. Warping Tension = (K x N) / (1693 x English Count) = 0.03 to 0.05 x Single Thread Strength 7.6. Sizing Calculations: Length meter in 1.094 × Total × Ends Warp weight (in Kg) = 1. 840 . 2 204 Warp Count × × Sized warp weight Un - - Sized warp weight. Size pick %age up 100 = × 2. Un - sized warp weight. 3. Weight of size = Warp Weight x Size pick up % Sized Warp Length Un − - Sized Warp Length. Stretch %age 100 = × 4. Un - sized warp Length. Total Ends Warp length in yards × Sized yarn Count = 5. Sized warp weight (lbs.) × 840 Wt. of Sized Yarn - Wt. of Oven Dried Yarn 100 × 6. % Moisture Content = Wt. of Sizd Reading Yarn − Delivery counter Feed Counter Reading 100 × 7. % Stretch = Feed C Counter Reading 840000 D × × 8. % Droppings on loom = 454 Y N P × C = English Count N = Number of Ends × D = Dropping in gms. Y = Length woven (yds.) P = % size add on Amount of material size issued Amount - of size added yarn on 100 × 9. Invisible Loss % = Amount = = = of size 2.0 kg / kg of sized yarn 0.3 kg / kg of liquor 0.2 kg / kg of yarn = issued Steam Consumption (Sizing M/c) 10. Max. Speed of machine (meters / min) 1000 Cylinder of No. × (Cooker) (Sow box) English Count × Number of Ends No. of Ends 0.6 × 11. Wt. Of Warp in gms / mtr = English Count 7.7. Weaving Calculations

  5. 1. Reed Count It is calculated in stock port system. No. of dents in 2 inches is called Reed Count EPI Reed count = 1 Weft crimp %age + 2. Reed Width 100 weft + crimp %age Reed Width Cloth widt h = × 100 3. Crimp %age Warp length Cloth - length Warp Crimp %age 100 = × Cloth length Weft length - Cloth widt h Weft crimp %age 100 = × Cloth widt h 4. Cloth Cover Factor EPI Warp cover factor = 1. Warp Count PPI Weft cover factor = 2. Weft count Wp.C.F. Wt.C.F. × Cloth cover factor Wp.C.F Wt.C.F = + − 3. 28 5. Maximum EPI for particular count 14 × Count 1. For plain fabrics = 4 Count 28 × × 2. For drill Fabrics = 6 5 Count 28 × × 3. For satin fabrics = 7 Ends / repeat / 1 yarn diameter × 4. Other design = No. of intersecti repeat / ons ends / repeat + 1 5. Yarn diameter. = 28 Count ×

  6. 6. Weave Density Ends / cm Tex K × × a) Warp Density = = < 250 Picks / = < 350 cm Tex K × × b) Filling Density = (Warp dencity - 100) × F.D. - 100 50 + c) Weave Density = (Weft dencity 100) - F.D. × - 100 d) Effective weave density = W. D x K of loom width x K of Design = < 72 Wp / filling - K Loom Width - K Cotton = 1.00 140 cm - 0.99 Polyester/Cotton = 1.03 180 cm - 1.00 Viscose Filament = 1.17 190 cm - 1.01 Polyester Filament = 1.22 220 cm - 1.02 250 cm - 1.08 330 cm - 1.15 360 cm – 1.20 Weave Design - K Plain1/1 = 1.00 Twill 1/2 = 0.87 Matt, Gabardine 2/2 = 0.82 Drill 1/3 = 0.77 Satin 1/4 = 0.69 7. To change the count and number of thread / inch, keeping the same denseness of the fabric: 1. To change the EPI Without altering the denseness: given in EPI cloth Warp count expected in cloth × EPI in Exp. Cloth = Warp count given in cloth 2. To change the count without altering the denseness:   2 EPI in exp. Cloth     Count in Exp. Cloth Count given in cloth = × given in EPI cloth

  7. 8. Warp requirement to weave a cloth Total ends 1.0936 × 453.59 × crimp% × Warp weight gms/mtrs in Waste%age = × a. Count x 840 inches in R.S. 453.59 x x PPI Weft Weigh gms/mtrs in t Crimp %age Waste%age = × × b. Count x 840   Cloth length in mtrs Weft wt. x Weft kgs in count x 1848 0.9144 x     = c. with the given weft weight inches in S. R. x PPI For Silk and Polyester Total ends Count × (Denier) Warp weight gms/ in mtrs Crimp% Waste × %age = × i. 9000 inches in RS PPI × Count × (Denier) Weft weigh gms/ in t mtrs % Waste %age = × × Crimp ii. 9000 Allowance for count in Bleached and Dyed Fabric: ⇒Count becomes 4% ⇒FinerDyed counts become max 6% Coarser 9. Fabric production calculation Motor pully diameter 1. Loom Speed Motor RPM = × Loom pully diameter Actual Production 2. Loom Efficiency %age 100 × = Calculated Production Yarn weigh Yarn weigh Dryed - t t 3. Moisture Regain %age 100 × = × Yarn weigh Dryed t Yarn weigh Yarn weigh Dryed - t t 4. Moisture Content %age 100 × = × Yarn weigh t

  8. Moisture Regain% Moisture Content% 7.83 12.10 9.91 9.91 14.50 3.78 Type of Yarn Cotton Jute Silk Rayon, Viscose Wool Nylon Polyester 8.50 13.75 11.00 11.00 17.00 4.20 Total ends Tape × length meter. in 5. Warp weight in Kg. = 1693.6 Warp × Count RS in centi - meters Cloth × Length meters in PPI × 6. Weft weigh in t Kg. = 4301.14 Weft × Count   EPI PPI 7.   Cloth weig GSM in ht 25.6 × = + Warp Count Weft Count GSM (Grams Sq.Meter) per 8. (Ounze) Oz. per Sq. Yard = 34 10. Material measurement: To calculate the length of any rolled fabrics, this formula gives the nearest accuracy. d) (D d) (D 0.0655 + − L = t Where L = Length of material (Feet) t = Thickness of fabrics (inches) D = Outside diameter (inches) d = Inside diameter (inches) 11. Weight of yarn in a cloth: The weight of cloth manufactured on looms depends upon the weight of yarns in the warp and weft: ends/inch, picks/inch and the weight of size on the warp. Therefore, Cloth weight = Weight of warp + Weight of weft + Weight of size (All in lbs.) Total No. of Ends Tape Length in Yds. × Where as Weight of warp in lbs. = 840 Warp Yarn Count × Also Weight of weft in lbs.= Cloth of Length (Yds) Picks inch / in Cloth Reed Width (inch) × × 840 Weft Yarn Count ×

  9. 7.8. YARN QUALITY & OTHER PARAMETERS 1. Yarn Appearance: The Visual Effect obtained by viewing a sample of yarn wound with a designated traverse on a black board of designated size. ♦ Nep: a tightly tangled mass of unorganised fiber ♦ Slub: an abruptly thickened place of yarn ♦ Thick place: a yarn defect where the diameter is greater than the adjoining segments and extending for 6 mm ♦ Thin Place: a yarn segment where the diameter is 25% lesser than the average diameter of yarn ♦ Fuzz: Untangled fibers that protrude from the surface of the yarn ♦ Bunch: a yarn segment not over 6 mm in length that shows abrupt increase in diameter caused by more fibers matted in this particular place ♦ Method: yarn wound on hylam black boards wound for fixed wraps per inch as per count compared with standard reference boards. ♦ Grades: Above ‘A’ to below ‘D’ - The imperfections increase from Grade ‘A’ and the maximum in grade ‘D’. Average index of five boards of five graders. 2. Yarn Evenness: ♦ Unevenness: Variation in the linear density of a continuous strand or of a portion of a strand. ♦ Apparatus: Uster–Evenness Tester ♦ Principle: Difference in the capacitance variation. Lower the Count lower the Imperfections. One km of yarn is run through two capacitance plated at specific speed (fixed as per the count). The capacitance variation is integrated and expressed as % unevenness (U%). The imperfections are counted and are reported per kilometer. 3. Linier Density of Yarn: ♦ Expression of the fineness of Yarn ♦ A number indicating the mass per unit Length or the length per unit mass of Yarn ♦ Direct system: Denier, Tex (Weight Of Unit Length) ♦ Indirect System (Units of Lengths) per (Units of weights)

  10. 4. Count Test – Apparatus ♦ Wrap reel ♦ Balance ♦ 120 yards of yarn / 100 meters of yarn wound in a wrap reel and weighed . ♦ From the weight, the count is calculated. 5. Single Thread Strength Testing ♦ Force Required to break a single strand of yarn of unit length ♦ Apparatus - Single thread Strength Tester ♦ RKM ♦ %Elongation 6. Lea Stength Testing ♦ Lea Breaking Strength ♦ The Force required to break one lea ♦ Unit –pounds ♦ Count Strength Product ♦ Apparatus –Lea Tester 7. Principles Of Tensile Testing ♦ Constant Rate of Loading: The Rate of change of Load is constant – Uster Dynamat ♦ Constant rate of Traverse: The pulling clamp moves at a constant rate – Lea – Pendulum tester ♦ Constant rate of Extension:Rate Of change of Specimen length is constant – Statmat 8. Twist Testing ♦ Direction Twist ♦ S –Twist: When Held in vertical position, the spiral confirm in slope to the central position of the letter ‘S’ ♦ Z –Twist: When Held in vertical position, the spiral confirm in slope to the central position of the letter ‘Z’ ♦ No of Turns (Twists) per Unit length ♦ Single Twist

  11. ♦ Double Twist ♦ Twist Multiplier ♦ Apparatus: Twist Tester ♦ Direct Method ♦ Indirect Method 7.9. Analysis Of Cloth Sample: On analysing a sample of cloth made from cotton; rayon, silk or flax with view of its reproduction produced thus: - 1. Record whether a fabric is in the grey or the finished state. 2. Determine which threads constitute warp and which weft. 3. If in grey, test for the presence of size material by staining with iodine, when the starch in the size warp turns deep blue in colour, the weft being unaffected. 4. Examine for direction of spinning twist in the yarns, and also if either set of threads is two-fold yarn. If crepe yarns have been used it may be necessary to test for amount of twist present. 5. Count the ends and picks per inch in the fabric. If more than 2 warps or wefts are used, find the number per inch of each yarn type used. 6. Test the yarns for Regain i.e. how much longer they are out of the cloth than the length of the sample from which they were abstracted. By this means we can estimate the length of warp required to give the length to cloth and from the weft regain we can estimate the length in Reed or length of each pick of weft. In weaving ordinary classes 10% of cotton goods warp regain between 4% and according to the structure, while the weft regain is usually about 5%. These figures apply to grey cloths only. In finished goods, the regain will differ according to the nature of the finished applied. Very often the length of the cloth is increased and its width reduced on finishing, hence the warp regain may be as low as 1% to 4% while the weft regain may be 8% to 10 %. “Rigmel” finished and “Sanforising” are finishing processes in which the fabric is pre-shrunk both in warp and weft directions, the advantage being that the fabric, when made into a garment, will retain its shape: it will not shrink in the laundering. When analysing these materials regains of 8% to 10% will probably be found in both warp and weft. 7. Test the yarns for counts of warp and weft (The count of the yarn is the number of length units required to weight on gain). In a grey sample the warp will probably be sized yarn and the count recorded will be the sized count. This should be corrected by making a second test after thoroughly washing the fabric to remove all size and

  12. filling materials. If the sample is a bleached, dye, or printed cloth, the counts of warp and weft will be affected counts test then made, allowing about 5% in bleached count = 20s grey count: 38s bleached = 36s grey count. 8. Analyse the sample for weave details i.e. whether plain, twill, satin, or some other weave, and proceed to develop the draft and peg plan when necessary. 9. When analysing the sample containing rayon yarns, it is important to test for type of rayon i.e. Viscose, Cuprammonium or Cellulose Acetate, i.e. number of filaments comprising the rayon thread must be countered and the yarn exactly matched to obtain true reproduction of the sample. If the fabric is a coloured woven material, such as a poplin shirting or a zephyr check, the warp and weft patterns must be abstracted. For the ordinary kinds of cotton fabrics the contraction during weaving makes the cloth stand about 4 ends per inch closer in the cloth than in the reed and there is a gain of about 2 picks per inch from the loom to the warehouse table. Thus if a cloth is required to the following dimensions: 36 inch wide, 120 yards long, 72 ends / 66 picks per inch, 34s warp, 30s weft, plain weave – the making particulars would be : warp length 126 yards : ends per inch in reed, 68 : pick wheel on loom, 64 : pure warp ends – 36 x 72 = 2592 plus selvedge allowance say 30 extra ends = 2622 ends width in reed 38.2 in. When estimating the grey or loom particulars to reproduce a given finished sample of cloth, experience in the handling of that type of cloth, both in the grey and finished states, is necessary. No general rule can be laid down to cover all classes of goods, careful measurement of regains will, in most cases, be of great assistance in this work.