Atomic Layer Deposition for SCRF

DESCRIPTION

Atomic Layer Deposition for SCRF. J. Norem ANL/HEP. RF in the MTA 11/15/10. Atomic Layer Deposition. Atomic Layer by Layer Synthesis Method similar to MOCVD Used Industrially Semiconductor Manufacture for “high K” gate dielectrics “Abrupt” oxide layer interfaces

1 / 9

Download Presentation
Télécharger la présentation

Atomic Layer Deposition for SCRF

An Image/Link below is provided (as is) to download presentation Download Policy: Content on the Website is provided to you AS IS for your information and personal use and may not be sold / licensed / shared on other websites without getting consent from its author. Content is provided to you AS IS for your information and personal use only. Download presentation by click this link. While downloading, if for some reason you are not able to download a presentation, the publisher may have deleted the file from their server. During download, if you can't get a presentation, the file might be deleted by the publisher.

E N D

Presentation Transcript


  1. Atomic Layer Deposition for SCRF J. Norem ANL/HEP RF in the MTA 11/15/10

  2. Atomic Layer Deposition • Atomic Layer by Layer Synthesis Method similar to MOCVD • Used Industrially • Semiconductor Manufacture for “high K” gate dielectrics • “Abrupt” oxide layer interfaces • Pinhole free at 1 nm film thicknesses • Conformal, flat films with precise thickness control • Electroluminescent displays • No line of sight requirement • Large area parallel deposition • Parallel film growth technique; Inside of large tubes can be done at once.

  3. Ellipsometry Atomic Force Microscopy 4000 3500 3000 2500 Thickness (Å) 2000 1500 1000 Seagate, Stephen Ferro 500 0 • RMS Roughness = 4 Å (3000 Cycles) • ALD Films Flat, Pinhole free 0 500 1000 1500 2000 2500 3000 Flat, Pinhole-Free Film AB Cycles • Film growth is linear with AB Cycles ALD Reaction Scheme • ALD involves the use of a pair of reagents. • each reacts with the surface completely • each will not react with itself • This setup eliminates line of site requirments • Application of this AB Scheme • Reforms the surface • Adds precisely 1 monolayer • Pulsed Valves allow atomic layer precision in growth • Viscous flow (~1 torr) allows rapid growth • ~1 mm / 1-4 hours • No uniform line of sight requirement! • Errors do not accumulate with film thickness. • Fast! ( mm’s in 1-3 hrs ) and parallel • Pinholes seem to be removed. • Bulk

  4. Apparatus • Hot wall reactor (RT-400 C) • Always coat the wall – now it will be useful

  5. Oxide Nitride Element Ph/As C F S/Se/Te Demonstrated ALD A/B Reactions Element

  6. 150 nm Aerogels coated with W • Conformal Coating and “sharp” points • Aerogels are low density nanoporous materials consisting of bundles of nm scale filaments • ALD can be used to deposit W metal atomic layer by layer on this filaments Overall Reaction: WF6 + Si2H6 → W + products 10 nm filaments

  7. 3 c W 7 c W 80 nm 80 nm Microscopy of W-Coated Carbon Aerogels SEM TEM • Aerogel filament diameter increases with ALD W Cycles

  8. Higher-TcSC: NbN, Nb3Sn, etc Nb, Pb Insulating layers Goal of ALD SCRF • Build “nanolaminates” of superconducting materials • ~ 10- 30 nm layer thicknesses

  9. Conclusions • ALD is an intriguing synthesis technique with many useful properties • Conformal coating means increased radius of curvature • Parallel (non-line of sight) method • Flat samples directly map to complex shape samples even with high aspect ratios • Layer by layer growth on complex shapes • Useful for higher field gradients in SRF and NCRF