An Image/Link below is provided (as is) to download presentation Download Policy: Content on the Website is provided to you AS IS for your information and personal use and may not be sold / licensed / shared on other websites without getting consent from its author. Content is provided to you AS IS for your information and personal use only. Download presentation by click this link. While downloading, if for some reason you are not able to download a presentation, the publisher may have deleted the file from their server. During download, if you can't get a presentation, the file might be deleted by the publisher.

E N D

Presentation Transcript

Playing audio...

  1. Atomic Layer Deposition - ALD Introduction Example of Al2O3 ALD at MiNaLab Deposition materials Advantages and disadvantages Summary

  2. Atomic Layer Deposition Excellent thickness controll and step coverage Self-limited process Developed in 1974 First industrial use: electrolumenicent panels

  3. Some opportunities of ALD • Nanolaminate: ZrO2 and SiO2 • Coated deep trench structure

  4. ALD of Al2O3 on Si

  5. ALD at MiNaLab Al2O3, ZnO, TiO2 Thickness: sub nm - 400 nm

  6. ALD – deposited materials • Oxides (Al2O3, ZnO, TiO2, HfO2, HfSiO, La2O3, SiO2, Ta2O5) • Nitrides (TiN, TaN, SiN, HfN, AlN) • Sulfides (ZnS) • Metals (Cu, W, Pt, Ru)

  7. Applications • High quality photonics • Thin solarcells laminate => • Thin gate oxides with high dielectric constant • Diffusion barriers and passivation of active layers • Single metal coating for catalysts

  8. Advantages of ALD • Low temperature deposition is possible • Excellent step coverage and reproducibility • High density film and no pinholes • Easy to scale up

  9. Disadvantages of ALD • Expensive equipment • Critical adjustment of the flow: too much flow => clogging of valves too low flow => under-performance

  10. Summary ALD is excellent for: • Thin films • High density • Excellent stociometry controll • 3D structures • Large area substrates: no problem 