Atomic Force Microscope Nanoindentation/Scratching. Nanoindentation/Scratching. Elastic & plastic material properties are obtained from load-displacement data, but knowledge of the true area of contact is critical. sink-in. Load (µN). Stiffness, S:. (nm). pile-up.

1 / 7

Télécharger la présentation

Atomic Force Microscope Nanoindentation/Scratching

An Image/Link below is provided (as is) to download presentation Download Policy: Content on the Website is provided to you AS IS for your information and personal use and may not be sold / licensed / shared on other websites without getting consent from its author. Content is provided to you AS IS for your information and personal use only. Download presentation by click this link. While downloading, if for some reason you are not able to download a presentation, the publisher may have deleted the file from their server. During download, if you can't get a presentation, the file might be deleted by the publisher.

E N D

Presentation Transcript


  1. Atomic Force Microscope Nanoindentation/Scratching

  2. Nanoindentation/Scratching Elastic & plastic material properties are obtained from load-displacement data, but knowledge of the true area of contact is critical. sink-in Load (µN) Stiffness, S: (nm) pile-up

  3. Indentation is Possible With F/D Curves Tip moving in Tip moving out C D A F B E B A C F E D

  4. AFM Nanoindenting Problems With AFM:a) The probe geometry (area) is not know, not quantitative b) The probe motion is not horizontal at contact.

  5. AFM Scratching When Scratching With the AFM, there is a torsion on the cantilever so the probe area changes.

  6. Nanoindentation Characterization The AFM is ideal for characterizing nanoindents and nano scratches in a surface. AFM Image of nanoindents in a surface.

  7. Summary • All AFM instruments can create nanoindents and nanoscratches in a surface. • The technique is not quantitative because the probe/surface angle is not characterized • The AFM is useful for characterizing nanoindents and nanoscratches.