An Image/Link below is provided (as is) to download presentation Download Policy: Content on the Website is provided to you AS IS for your information and personal use and may not be sold / licensed / shared on other websites without getting consent from its author. Content is provided to you AS IS for your information and personal use only. Download presentation by click this link. While downloading, if for some reason you are not able to download a presentation, the publisher may have deleted the file from their server. During download, if you can't get a presentation, the file might be deleted by the publisher.

E N D

Presentation Transcript


  1. SAMARISCreep test Meeting at TRL 2-3 March 2005

  2. Time schedule • Sample reception • LAVOC cores December 2004 • DRI slabs February 2005 • Test program • Sample preparation (coring and cutting) February 05 • Density measurement • Creep test • At 50°C February-March 05 • At additional T°C to be discussed • Binder information ?

  3. Creep test conditions (1/2) • European standard PrEN 12696-25 • Method A: uniaxial cyclic compression test with confinement • Method B: triaxial cyclic compression test • British Standard BS 598-111 • Unconfined uniaxial loading test • Internal Shell protocol • Performed on the NAT • Sample size 100 mm Diam 60 mm Height • Normal stress 100kN • Temperature 50°C • Pulse time 0.2s loading + 1.8s rest

  4. Creep test conditions (2/2)

  5. Sample preparation • From LAVOC material Done • 2x9 cores 90mm diam (not 100mm) • Layer sawing in order to have • Surface layer 2x30mm thick • Base layer 60mm thick • From DRI material Under progress • 2 slabs • Coring • Layer sawing as for LAVOC

  6. Preliminary measurements (1/3) • Density measurement (for the time being for LAVOC only) • Require information on mix characteristics (density, composition, …) • Slight difference between base and surface layers • Scattering of results (higher for surface than base) Impact of test results

  7. Preliminary measurements (2/3)

  8. Preliminary measurements (bis)

  9. First creep test result for LAVOC • Base layer • Excellent behaviour • Longer test required • Surface layer • Lower behaviour • Breakdown of certain sample

  10. Next step • Creep test on the DRI material at 50°C • Further information on mixture • Coefficient calculation • Binder data (viscosity of fresh binder) ? • To be discussed • Test at another temperature? Other conditions?