Wafer Preparation

Wafer Preparation. Challenge in epitaxial growth : - Achieving defect free films at low temperate. More than half of the yield loss is due to contamination such as organic and metallic impurities. -------------- surface preparation is important. Wafer Preparation.

liko
Télécharger la présentation

Wafer Preparation

An Image/Link below is provided (as is) to download presentation Download Policy: Content on the Website is provided to you AS IS for your information and personal use and may not be sold / licensed / shared on other websites without getting consent from its author. Content is provided to you AS IS for your information and personal use only. Download presentation by click this link. While downloading, if for some reason you are not able to download a presentation, the publisher may have deleted the file from their server. During download, if you can't get a presentation, the file might be deleted by the publisher.

E N D

Presentation Transcript


  1. Wafer Preparation • Challenge in epitaxial growth : - Achieving defect free films at low temperate. • More than half of the yield loss is due to contamination such as organic and metallic impurities. -------------- surface preparation is important

  2. Wafer Preparation • Surface preparation prior to epi growth generally consist of 2 part : (1) ex-situ clean : RCA cleaning (2) in-situ clean : high temperature H2 annealing

  3. RCA and HF dip • RCA Clean : (1)Removing the organic and metallic impurities from the silicon surface by oxidizing the silicon surface (2) Forming complexes with the contaminants,which become water-soluble. .

  4. RCA Clean 標準步驟 • 1. GP4振10~15 分鐘 (GP : H2O = 1 : 15 ) (此步驟通常不做) 2. ACE 振 10~15 分鐘, 沖 DI water 5分鐘 3. H2SO4 : H2O2 = 2 : 1 泡15~20 分鐘 , 沖 DI water 5分鐘 (H2SO4 can remove organic.) 4.Dip HF 至不沾水, 沖 DI water 5分鐘

  5. RCA Clean 標準步驟 (SC1) 5. NH4OH : H2O2 : H2O = 0.05 : 1 : 5 煮 (先煮水) 15~20分鐘 , 沖 DI water 5分鐘 (remove particle by forming chemical oxide) (SC2) 6. HCL : H2O2 : H2O = 1 : 1 : 6 , 煮15~20分鐘 (先煮水) , 沖 DI water 5分鐘 (remove metal ) 7. Dip HF 至不沖水 ,沖 DI water 數秒

  6. RCA after with HF last • After the RCA clean - the silicon surface is left passivated with a chemical oxide ,which protect the surface against recontamination • HF dip : Removing the chemical oxide and the native oxide to achieve the atomically clean silicon surface

  7. RCA after with HF last • To accomplish low temperature epitaxy, one must have an atomically clean Si surface 1.The Si surface is Si-H terminated 2.Highly resistant to oxidation 3.May be exposed to room air for several minutes without significant oxidation HF clean

  8. After HF Dip • HF : DI =1 : 100 H passivation H H H H H H H O H H H

  9. H2 Prebake • If the temp. of H2 bake is higher than 1000°C --------no HF etch is necessary And ------surface is better than HF dip followed by a H2 pre-bakes at 900°C or less.

  10. High Temp. Effect of H2 Prebake • But high temp. may causes

  11. Low Temp. Bake • The commercial UHCVD systems that are capable of bake temperature (EpiGress) usually require 20 minutes at 800ºC to have an O & C free interface. but the problem is : The EpiGress takes a lot time to ramp up to 800ºC then cool to a deposition temperature of 550-650ºC ------- Not too good for throughput

  12. Low Temp. Bake • ASM has developed a novel hydrogen prebake that has the potential lower the bake temperatures (below 700ºC). • If this novel technique is combined with plasma NF3 chamber cleaning at say the benefits to throughput would also be significant

  13. Water Vapor and Bake Conditions • Water vapor is the most persistent contaminate in any vacuum system • The effectiveness of the bake at a given temperature is directly proportional to the water and oxygen background in a given system

  14. Surface Oxide Formation by Moisture

  15. SiGe Epitaxial growth • Choosing a Growth Temperature : - tc(critical thickness) is the most important factor - IF the critical layer thickness for a given Ge fraction is exceeded , misfit dislocation injection occurs.

  16. Critical Thickness

  17. Metastable state

  18. Metastable state • Growth conditions At low Temp.(625ºC) Surface reaction limited Nonthermal equil. • Fewer dislocations than expected ,when t>tc

  19. Misfit dislocation • The thickness of SiGe growth >tc The film relaxs Misfit dislocation • This relaxation is catastrophic for SiGe HBT application

  20. Dislocation number • The number of dislocation in non-selective area

  21. Dislocation number • The number of dislocation in the selective area

  22. Enhancement Factor (EF)

  23. Si0.8Ge0.2 • Two samples were studied (A) 150nm with hole edge aligned with {100} direction (B) 200nm with hole edge aligned with {100} direction

  24. Si0.8Ge0.2 {110} {100}

  25. Threading dislocation • Threading dislocation in HBT

  26. Threading dislocation

  27. Gradual relaxed buffer

  28. Strain after anneal

  29. Deposition temperature • Once this critical thickness guideline is satisfied : Deposition temperature(T) The film quality for the epitaxial film

  30. Film Quality when T decrease, the silane flow must decrease also. ex: T : 700ºC ; 100% silane : 50sccm------will deposit a specular high quality film. but T : 600°C ; 100% silane :50sccm-----the film beome hazy

  31. Film Quality • Faceting/Conformality - Lower temperature and the resultant lower growth rates result in less faceting and improved conformality • Poly/Si growth ratio ----- for customers who use a field oxide, depending on temp, this ratio can vary. - Low T favors Si(single crystal) growth - High T favors poly growth

  32. Dichlorosilane(DCS) • Dcs(SiH2Cl2 )is the only one that has been applied to the growth of SiGe epitaxial layers - SiCl2 on the surface is then thought to react with hydrogen to form HCL and a silicon adatom

  33. Advantage of DCS over silane • Specular defect free surface -----Superior surfaces are evident with DCS even when processing atextremely low temperaturesas a result ofthe HCL released in the decomposition. • Temperature : DCS : 700C , silane : 600C. • Safety -----silane is explosive and highly pyrophoric